High-Speed Nanoindentation and Local Residual Stress Analysis for Cut Edge Damage in Complex Phase Steels for Automotive Applications

with No hi ha comentaris
  • Ortiz-Membrado, L., Parareda, S., Casellas, D., Jiménez-Piqué, E., & Mateo, A. (2025). High-Speed Nanoindentation and Local Residual Stress Analysis for Cut Edge Damage in Complex Phase Steels for Automotive Applications. Metals, 15(6), 651. https://doi.org/10.3390/met15060651